Brand:
SATItem NO.:
SATOF-25x16x10-980Order(MOQ):
3000Payment:
EXWProduct Origin:
ChinaColor:
CustomizedShipping Port:
Shenzhen/ Huizhou/ HongkongLead Time:
7-15 DaysSAT Nanocrystalline Epoxy Resin Magnetic Toroidal Core
The epoxy resin coated SAT tape-wound toroidal cores made of nanocrystalline or amorphous magnetic material, perform higher permeability, lower core loss and higher energy switching efficiency than ferrite and permalloy ones. It’s the best core material for common mode choke, smart energy meter, coil, toroidal transformer and electronic components. SAT magnetic toroidal cores make electronic components smaller, lighter and cleaner.
The Specification of Epoxy Resin Magnetic Toroidal Cores
Core design |
Toroidal core |
Core for common mode choke |
251610 |
Nominal Dimensions |
25x16x10mm |
Core Material |
SAT1K101 |
Type of Finish |
Plastic box / silicon rubber |
Rated Dimensions |
Afe=0.36m² lFe=6.45cm mFe=17.5g |
Final Inspection |
Magnetical Test Measurement at room temperature (AQL 0,65) Inductance test without DC-magnetisation |
7.1 Setting values: f=100KHz / 0.3 14mA Specified value: 2.3µH≤ AL ≤4.5µH (Magnetic conductivity 3300≤ µ`3≤6400) |
Epoxy Resin Magnetic Toroidal Cores Features:
1. The operating temperature of toroidal cores with epoxy resin coating up to 120 °C
2. Cores with plastic casing for operating temperatures up to 130 °C
3. The toroidal shape provides higher permeability and lower core loss than ferrite and permalloy
4. Different permeability levels toroidal cores for electronic components are available
Please leave a message below for more details of magnetic toroidal cores product information.